Creep resisting steels, nickel and cobalt alloys

1.1   This European Standard covers the grades of wrought steels and alloys listed in Table 1 and Table 2, which are usually employed for components and equipment, for which the main requirement is their creep resistance under mechanical long-time stressing at temperatures above 500 C.
NOTE   Heat resisting grades given in EN 10095 [9] may also be used for similar applications if so agreed.
1.2   This European Standard specifies the technical delivery conditions for semi-finished products, for hot or cold rolled sheet/plate and strip, hot or cold formed (cold drawn) bars, rods, wire and sections.
1.3   The general technical delivery conditions specified in EN 10021:2006 apply in addition to the specifications of this European Standard, unless otherwise specified in this European Standard.
1.4   This European Standard does not apply to components manufactured by further processing the product forms listed in 1.2 with quality characteristics altered as a result of such further processing.
1.5   This European Standard shall not be used for aerospace and pressure purposes.
1.6   For steels and alloys with similar chemical composition, but intended for different applications, see the Bibliography.

Warmfeste Stähle, Nickel- und Cobaltlegierungen

1.1 Diese Europäische Norm gilt für die in den Tabellen 1 und 2 aufgeführten Sorten von Stählen und
Legierungen, die üblicherweise für Erzeugnisse verwendet werden, bei denen die Langzeitwarmfestigkeit
unter mechanischer Beanspruchung bei Temperaturen oberhalb 500 °C die Hauptanforderung darstellt.
ANMERKUNG Falls vereinbart, dürfen auch hitzebeständige Stähle nach EN 10095 [9] für ähnliche Anwendungen
verwendet werden.
1.2 Diese Europäische Norm legt die technischen Lieferbedingungen für Halbzeug, warm- oder kaltgewalztes
Blech und Band, warm- oder kaltgeformte (kaltgezogene) Stäbe, Walzdraht, gezogenen Draht und
Profile fest.
1.3 Zusätzlich zu den Angaben dieser Europäischen Norm gelten, sofern in dieser Norm nichts anderes
festgelegt ist, die in EN 10021 wiedergegebenen allgemeinen technischen Lieferbedingungen.
1.4 Diese Europäische Norm gilt nicht für die durch Weiterverarbeitung der in 1.2 genannten Erzeugnisformen
hergestellten Teile mit fertigungsbedingten abweichenden Gütemerkmalen.
1.5 Diese Europäische Norm darf nicht für Luft- und Raumfahrt- sowie Druckbehälteranwendungen benutzt
werden.
1.6 Für Stähle und Legierungen mit ähnlicher chemischer Zusammensetzung, jedoch anderem Verwendungszweck,
siehe Abschnitt Literaturhinweise.

Aciers et alliage à base de nickel et de cobalt résistant au fluage

1.1   La présente Norme européenne traite des nuances d'aciers et d'alliage corroyés énumérés dans les Tableaux 1 et 2 qui sont généralement employés pour la fabrication de pièces et de matériels, dont l'exigence principale porte sur la résistance au fluage lorsqu'elles subissent une contrainte de longue durée à des températures supérieures à 500 °C.
NOTE   Les nuances d'aciers réfractaires données par l'EN 10095 [9] peuvent, si cela fait l'objet d'un accord, être utilisées pour des applications similaires.
1.2   La présente Norme européenne spécifie les conditions techniques de livraison des demi-produits, des tôles/bandes et feuillards laminés à chaud ou à froid, des barres, du fil machine, des fils et des profils transformés à chaud ou à froid (étirés à froid).
1.3   Sauf spécification contraire dans le présent document, les conditions techniques générales de livraison spécifiées dans l'EN 10021 s'appliquent en plus des spécifications de la présente Norme européenne.
1.4   La présente Norme européenne ne s'applique pas aux éléments fabriqués par transformation ultérieure de produits énumérés en 1.2, qui aurait pour effet de modifier les caractéristiques de qualité de ces produits.
1.5   La présente norme européenne n'est pas destinée à être utilisée dans le cadre d'applications aérospatiales ou sous pression.
1.6   Pour les aciers et alliages ayant une composition chimique analogue mais destinés à d'autres applications, voir la bibliographie.

Jekla ter nikljeve in kobaltove zlitine, odporne proti lezenju

General Information

Status
Published
Publication Date
18-Mar-2008
Withdrawal Date
29-Sep-2008
Current Stage
9093 - Decision to confirm - Review Enquiry
Start Date
01-Nov-2012
Completion Date
01-Nov-2012

Relations

Buy Standard

Standard
EN 10302:2008
English language
46 pages
sale 10% off
Preview
sale 10% off
Preview
e-Library read for
1 day

Standards Content (Sample)


2003-01.Slovenski inštitut za standardizacijo. Razmnoževanje celote ali delov tega standarda ni dovoljeno.Jekla ter nikljeve in kobaltove zlitine, odporne proti lezenjuWarmfeste Stähle, Nickel- und CobaltlegierungenAciers et alliage a base de nickel et de cobalt résistant au fluageCreep resisting steels, nickel and cobalt alloys77.120.70Kadmij, kobalt in njune zlitineCadmium, cobalt and their alloys77.120.40Nikelj, krom in njune zlitineNickel, chromium and their alloys77.080.20JeklaSteelsICS:Ta slovenski standard je istoveten z:EN 10302:2008SIST EN 10302:2008en,de01-maj-2008SIST EN 10302:2008SLOVENSKI
STANDARDSIST EN 10302:2003/AC:2005SIST EN 10302:20031DGRPHãþD

EUROPEAN STANDARDNORME EUROPÉENNEEUROPÄISCHE NORMEN 10302March 2008ICS 77.120.01; 77.140.01; 77.150.01Supersedes EN 10302:2002
English VersionCreep resisting steels, nickel and cobalt alloysAciers et alliage à base de nickel et de cobalt résistant aufluageWarmfeste Stähle, Nickel- und CobaltlegierungenThis European Standard was approved by CEN on 10 February 2008.CEN members are bound to comply with the CEN/CENELEC Internal Regulations which stipulate the conditions for giving this EuropeanStandard the status of a national standard without any alteration. Up-to-date lists and bibliographical references concerning such nationalstandards may be obtained on application to the CEN Management Centre or to any CEN member.This European Standard exists in three official versions (English, French, German). A version in any other language made by translationunder the responsibility of a CEN member into its own language and notified to the CEN Management Centre has the same status as theofficial versions.CEN members are the national standards bodies of Austria, Belgium, Bulgaria, Cyprus, Czech Republic, Denmark, Estonia, Finland,France, Germany, Greece, Hungary, Iceland, Ireland, Italy, Latvia, Lithuania, Luxembourg, Malta, Netherlands, Norway, Poland, Portugal,Romania, Slovakia, Slovenia, Spain, Sweden, Switzerland and United Kingdom.EUROPEAN COMMITTEE FOR STANDARDIZATIONCOMITÉ EUROPÉEN DE NORMALISATIONEUROPÄISCHES KOMITEE FÜR NORMUNGManagement Centre: rue de Stassart, 36
B-1050 Brussels© 2008 CENAll rights of exploitation in any form and by any means reservedworldwide for CEN national Members.Ref. No. EN 10302:2008: ESIST EN 10302:2008

Applicable dimensional standards.25 Annex B (informative)
Technical information on creep resisting steels, nickel and cobalt alloys.26 Annex C (informative)
Preliminary reference data for creep strength to 1 % plastic strain and creep rupture strength.29 Annex D (informative)
Guideline values for the physical properties of creep resisting steels, nickel and cobalt alloys.42 Bibliography.46
1.3 The general technical delivery conditions specified in EN 10021 apply in addition to the specifications of this European Standard, unless otherwise specified in this European Standard. 1.4 This European Standard does not apply to components manufactured by further processing the product forms listed in 1.2 with quality characteristics altered as a result of such further processing. 1.5 This European Standard shall not be used for aerospace and pressure purposes. 1.6 For steels and alloys with similar chemical composition, but intended for different applications, see the Bibliography. 2 Normative references The following referenced documents are indispensable for the application of this document. For dated references, only the edition cited applies. For undated references, the latest edition of the referenced document (including any amendments) applies. EN 10002-1, Metallic materials - Tensile testing - Part 1: Method of test (at ambient temperature) EN 10002-5, Metallic materials - Tensile testing - Part 5: Method of testing at elevated temperature EN 10020:2000, Definition and classification of grades of steel EN 10021:2006, General technical delivery conditions for steels products EN 10027-1, Designation systems for steels - Part 1: Steel names EN 10027-2, Designation systems for steels - Part 2: Numerical system EN 10052:1993, Vocabulary of heat treatment terms for ferrous products EN 10079:2007, Definition of steel products EN 10163-2, Delivery requirements for surface condition of hot rolled steel plates, wide flats and sections - Part 2: Plate and wide flats EN 10168:2004, Steel products – Inspection documents – List of information and description EN 10204, Metallic products - Types of inspection documents EN 10221, Surface quality classes for hot-rolled bars and rods - Technical delivery conditions prCEN/TR 10261, Iron and steel - Review of
available methods of chemical analysis EN ISO 377:1997, Steel and steel products - Location and preparation of samples and test pieces for mechanical testing (ISO 377:1997) SIST EN 10302:2008

steels, nickel- or cobalt-alloys with a minimum of 8 % chromium, which are characterised by good mechanical behaviour at temperatures above 500 °C under long-range service conditions; i.e. primarily by creep strength to 1 % plastic strain or creep rupture strength during long-time stressing NOTE For supplementary information on creep resisting steels and alloys see Annex B. 4 Classification and designation 4.1 Classification Materials covered in this European Standard are classified according to their structure into:  martensitic steels;  austenitic steels;  nickel alloys; and  cobalt alloys. 4.2 Designation The names and numbers of the steels (see Table 1) were formed in accordance with EN 10027-1 and
EN 10027-2 respectively. NOTE Explanation on the designation of nickel and cobalt alloys (see Table 2).  name: The preceding chemical symbols indicate the main alloy elements and the figure immediately following indicates the average content of these alloys which is subsequently followed by the symbol for the other important alloying elements added.  material number: The structure is set out according to EN 10027-2 with the number 2 for the material group number. This material group comprises chemically resistant and high temperature or heat resistant nickel and cobalt alloys. SIST EN 10302:2008

5 Information to be supplied by the purchaser 5.1 Mandatory information ≤ The following information shall be supplied by the purchaser at the time of enquiry and order: a) quantity to be delivered; b) designation of the product form (e.g. bar or rod, strip or plate); c) where an appropriate dimensional standard is available (see Annex A) the number of the standard and the indications required by this, also the nominal dimensions and tolerances; d) type of material (steel, cobalt or nickel alloy); e) number of this European Standard (EN 10302:2008); f) name or number of the steel grade, nickel or cobalt alloy (see 4.2); g) if for the relevant material in the table more than one treatment condition for the mechanical properties is covered, the symbol for the desired heat treatment condition or work hardened condition; h) desired process route (see symbols in Table 5 and Table 6). 5.2 Options ≤≤ A number of options are specified in this European Standard and listed below. If the purchaser does not indicate his wish to implement any of these options,
...

Questions, Comments and Discussion

Ask us and Technical Secretary will try to provide an answer. You can facilitate discussion about the standard in here.