EN 13523-6:2002
(Main)Coil coated metals - Test methods - Part 6: Adhesion after indentation (cupping test)
Coil coated metals - Test methods - Part 6: Adhesion after indentation (cupping test)
This Part of EN 13523 defines terms of the procedure for determining the adhesion of an organic coating to a metallic substrate after indentation after slow deformation.
The resistance to cracking may also be evaluated.
Bandbeschichtete Metalle - Prüfverfahren - Teil 6: Haftfestigkeit nach Eindrücken (Tiefungsprüfung)
Dieser Teil von EN 13523 beschreibt das Verfahren zum Bestimmen der Haftfestigkeit einer organischen Beschichtung auf einem metallischen Substrat nach Eindrücken bei langsamer Verformung.
Die Widerstandsfähigkeit gegen Rissbildung kann auch bewertet werden.
Tôles prélaquées - Méthodes d'essai - Partie 6 : Adhérence après indentation (essai d'emboutissage)
La présente partie de l'EN 13523 décrit la méthode de détermination de l'adhérence d'un revêtement organique sur un support métallique après indentation et déformation lente.
La résistance à la fissuration peut également être évaluée.
Kovine, zaščitene po postopku coil-coating - Metode preskušanja - 6. del: Oprijem po globljenju (preskus elastičnosti)
General Information
Relations
Standards Content (Sample)
2003-01.Slovenski inštitut za standardizacijo. Razmnoževanje celote ali delov tega standarda ni dovoljeno.Bandbeschichtete Metalle - Prüfverfahren - Teil 6: Haftfestigkeit nach Eindrücken (Tiefungsprüfung)Tôles prélaquées - Méthodes d'essai - Partie 6 : Adhérence apres indentation (essai d'emboutissage)Coil coated metals - Test methods - Part 6: Adhesion after indentation (cupping test)25.220.60Organske prevlekeOrganic coatings17.040.20Lastnosti površinProperties of surfacesICS:Ta slovenski standard je istoveten z:EN 13523-6:2002SIST EN 13523-6:2003en01-januar-2003SIST EN 13523-6:2003SLOVENSKI
STANDARD
EUROPEAN STANDARDNORME EUROPÉENNEEUROPÄISCHE NORMEN 13523-6July 2002ICS 17.040.20; 25.220.60English versionCoil coated metals - Test methods - Part 6: Adhesion afterindentation (cupping test)Tôles prélaquées - Méthodes d'essai - Partie 6: Adhérenceaprès indentation (essai d'emboutissage)Bandbeschichtete Metalle - Prüfverfahren - Teil 6:Haftfestigkeit nach Eindrücken (Tiefungsprüfung)This European Standard was approved by CEN on 11 April 2002.CEN members are bound to comply with the CEN/CENELEC Internal Regulations which stipulate the conditions for giving this EuropeanStandard the status of a national standard without any alteration. Up-to-date lists and bibliographical references concerning such nationalstandards may be obtained on application to the Management Centre or to any CEN member.This European Standard exists in three official versions (English, French, German). A version in any other language made by translationunder the responsibility of a CEN member into its own language and notified to the Management Centre has the same status as the officialversions.CEN members are the national standards bodies of Austria, Belgium, Czech Republic, Denmark, Finland, France, Germany, Greece,Iceland, Ireland, Italy, Luxembourg, Malta, Netherlands, Norway, Portugal, Spain, Sweden, Switzerland and United Kingdom.EUROPEAN COMMITTEE FOR STANDARDIZATIONCOMITÉ EUROPÉEN DE NORMALISATIONEUROPÄISCHES KOMITEE FÜR NORMUNGManagement Centre: rue de Stassart, 36
B-1050 Brussels© 2002 CENAll rights of exploitation in any form and by any means reservedworldwide for CEN national Members.Ref. No. EN 13523-6:2002 ESIST EN 13523-6:2003
Cross-hatching deviceA single-bladed knife, very sharp to avoid any burrs. For coatings less than 60 µm in thickness, it is also possible touse a purpose-made cutting tool, capable of making a minimum of 6 parallel cuts.5.2
Pressing deviceApparatus in accordance with EN ISO 1520:2001, consisting essentially of:a) a steel die, of inside diameter (27 ± 0,05) mm, its contact surface with the test specimen being flat andpolished;b) a retainer ring, having its flat and polished surface in contact with the test specimen;c) a striker consisting of a polished steel sphere, of diameter (20 ± 0,05) mm with a maximum of 0,1 mmdisplacement from the axis of the die;d) a system, preferably hydraulic, allowing movement of the striker at a speed of (12 ± 6) mm/min.5.3
Ageing deviceThe ageing device shall consist of:a) a vessel, to contain boiling water, whose dimensions allow the complete immersion of the test specimen;b) a heating system.5.4
Pincers, the jaws of which shall be flat, blunt and having a width of at least 5 mm.5.5
Magnifying glass ´10.5.6
Transparent pressure-sensitive adhesive tape, 25 mm wide, with an adhesion strength of(10 ± 1) N per 25 mm w
...
Questions, Comments and Discussion
Ask us and Technical Secretary will try to provide an answer. You can facilitate discussion about the standard in here.