Abstract

This document specifies standard methods for avoiding galvanic corrosion in the design stage and for determining whether actual corrosion damage was caused by galvanic corrosion. It also specifies guideline for standard methods for suppressing galvanic corrosion. This document also provides guidance for predicting galvanic corrosion in different environments (e.g. in water and in atmospheric and soil environments) by numerical calculation based on polarization data. This document does not establish the grounds for indexes related to safety or the loss of functions of materials in actual use. However, this document can be used to estimate the function maintenance life and safety maintenance life of these materials in advance. The responsibility for using the guideline rests with the reader.

Status
Published
Publication Date
09-Aug-2026
Current Stage
6060 - International Standard published - 60 Publication
Start Date
10-Aug-2026
Due Date
10-Jul-2026
Completion Date
10-Jul-2026

Buy Documents

Standard

ISO 16364:2026 - Corrosion of metals and alloys — Guidelines for galvanic corrosion control

Release Date:10-Aug-2026
English language (16 pages)
sale 15% off
Preview
sale 15% off
Preview
Standard

ISO 16364:2026 - Corrosion des métaux et alliages — Lignes directrices pour le contrôle de la corrosion galvanique

Release Date:10-Aug-2026
French language (16 pages)
sale 15% off
Preview
sale 15% off
Preview

ISO 16364:2026 is an International Standard from ISO on guidelines for galvanic corrosion control in metals and alloys. It gives designers, corrosion engineers, test personnel, and quality teams standard methods for avoiding galvanic corrosion in the design stage, judging whether observed damage was caused by galvanic corrosion, and suppressing it by structural, material, surface, environmental, or electrochemical measures. It also gives guidance for predicting galvanic corrosion in water, atmospheric, and soil environments from polarization data.

What does ISO 16364:2026 specify?

ISO 16364:2026 specifies a practical approach for controlling galvanic corrosion across design, investigation, prediction, and mitigation. It is organized into a short main body - Scope, Normative references, Terms and definitions, General principles, and Test report - plus three informative annexes that give visual, calculation, and test examples.

The scope is narrow in one important way: ISO 16364:2026 is a guideline for control and assessment, not a basis for safety or functional-loss indexes in actual use. At the same time, it can be used to estimate function maintenance life and safety maintenance life in advance, so it is useful when a team needs an engineering judgment before service.

AnnexWhat it covers
Annex AAn example schematic diagram of corrosion potential, including practical metal and alloy behavior in seawater and in other electrolytes
Annex BAn example calculation of galvanic corrosion using numerical methods and electrochemical boundary conditions
Annex CAn example galvanic corrosion test method, including typical test conditions and evaluation approaches

What are the key requirements of ISO 16364:2026?

ISO 16364:2026 is built around a flow-based method: first identify whether a galvanic couple exists, then decide whether the environment allows galvanic action, then choose a prevention or suppression measure, and finally confirm the outcome by test or analysis. In practice, that means the document is useful both for new designs and for troubleshooting damage in service.

Identify the galvanic couple and the electrolyte

Clause 4.2.2 requires checking whether dissimilar conductive materials are electrically connected, including indirect continuity through wiring or other conductive paths. If there is no electrical continuity, galvanic corrosion between those materials does not occur.

Clause 4.2.3 then requires checking whether the same materials also share a common electrolyte. This matters because the electrolyte closes the circuit needed for galvanic corrosion. The clause also points out that condensation can create intermittent electrolyte conditions, so the reader should consider whether moisture can appear even if it is not always visible.

Check whether the structure accelerates corrosion

Clause 4.2.4 asks whether the pair forms a corrosion-accelerating structure. It highlights the importance of potential difference, cathode-to-anode area ratio, and electrolyte resistance. In practice, a small anodic area against a large cathodic area, or a more conductive electrolyte, can increase attack on the anodic material.

Use design changes, prediction, or testing to judge the risk

Clause 4.2.5 allows the design to be changed after a data search, predictive calculation, or accelerated testing. The document names the finite element method (FEM) and the boundary element method (BEM) as calculation approaches, and it also describes salt spray tests, cyclic corrosion tests, galvanic current measurement with a zero-shunt ammeter, and electrochemical testing using the constant potential polarization method set to the coupling potential. In practice, this gives teams several ways to estimate corrosion amount and rate before committing to a final design.

Choose a suppression method in a practical order

Clause 4.3 presents suppression methods as a selection flow, and it notes that some options can be used in parallel. The choice should consider degree of effect, economy, convenience, and practicality.

The main options are:

  • change the contact structure, for example by insulating the mating surfaces or blocking electrolyte access
  • change the material combination, for example by replacing one material with a non-conductive or non-metallic material or by using similar materials
  • change the surface, for example by coating or plating
  • change the environment, for example by reducing humidity, removing aggressive species, or adding a corrosion inhibitor
  • use electrochemical protection, including cathodic protection or sacrificial anodes where suitable

In practice, this means the document is not limited to one fix. It guides the reader to the least disruptive measure that can be confirmed by test.

Confirm the effect before closing the issue

Several subclauses in 4.3 say to confirm the corrosion-protection effect by corrosion test. That is important because a theoretical fix may fail if coating defects, structural limits, or environmental conditions remain. ISO 16364:2026 therefore treats verification as part of the control process, not an afterthought.

Report the work in a traceable way

Clause 5 requires a report that records the materials, environment, coating details, additives, cathodic protection details, the standard used, the method used, the results with a reference to the calculation clause where relevant, the evaluation method for determining whether the damage was caused by galvanic corrosion, any deviations, unusual observations, and the test date. For a buyer, lab, or auditor, this is the part that makes the conclusion traceable.

What terms does ISO 16364:2026 define?

  • corrosion potential - The potential measured when materials A and B are immersed separately in the relevant electrolyte; the document distinguishes noble and base potential, which helps compare which material is more likely to act as the anode.
  • coupling potential - The potential measured when materials A and B are electrically short-circuited while in contact with the electrolyte; this is useful when assessing the driving force for galvanic action in the coupled state.
  • electrolyte - An ionically conductive liquid or solid medium covering the surfaces of both materials; without it, galvanic current cannot pass.
  • area ratio - The ratio between the area of the base-potential material and the noble-potential material; this matters because a small anode against a large cathode can accelerate attack.
  • corrosion accelerate structure - A structure that increases corrosion mass loss on the base side through anodic reaction; the document uses this to describe geometries or conditions that make galvanic corrosion worse.

Who uses ISO 16364:2026?

ISO 16364:2026 is aimed at people who design, assess, test, or troubleshoot structures made from dissimilar materials. It is relevant in electronic components, automobiles, aircraft, plant systems, and infrastructure, where multi-material designs are increasingly common.

Typical users include design engineers choosing material pairs, corrosion engineers evaluating failure mechanisms, test laboratories running galvanic corrosion tests, quality managers documenting conclusions, and maintenance or reliability teams estimating service life and repair risk. A buyer or specifier can also use it to check whether a proposed design has a clear galvanic corrosion control plan.

Which standards are used with ISO 16364:2026?

ISO 16364:2026 cites several related standards in its informative material and bibliography that help with testing or comparison work.

  • ISO 7441 - used in Annex C as a typical standard for determining bimetallic corrosion in atmospheric exposure corrosion tests.
  • ISO 21746 - used in Annex C for galvanic corrosion tests of carbon fibre reinforced plastics (CFRPs) related bonded or fastened structures in artificial atmospheres.
  • ASTM G71 - used in Annex C as a guide for conducting and evaluating galvanic corrosion tests in electrolytes.
  • ISO 9227 - cited with salt spray tests in Annex C as a reference for artificial atmosphere testing.
  • ASTM G82 - cited in the bibliography as a guide for developing and using a galvanic series for predicting galvanic corrosion performance.

What does the ISO 16364:2026 document contain?

ISO 16364:2026 contains a flow-based method for design review, damage assessment, and suppression of galvanic corrosion. It includes a general principle section that explains the galvanic current path and how corrosion rate rises with current density.

The informative annexes add practical support. Annex A gives an example corrosion-potential diagram for practical metals and alloys, including seawater behavior and notes on how the noble/base order can change with environment and time. Annex B sets out calculation examples with mass transfer, charge balance, polarization boundary conditions, and numerical methods such as FEM and BEM. Annex C provides a test-method example with typical conditions such as specimen form, coupling method, temperature, duration, and evaluation approach.

Buy Documents

Standard

ISO 16364:2026 - Corrosion of metals and alloys — Guidelines for galvanic corrosion control

Release Date:10-Aug-2026
English language (16 pages)
sale 15% off
Preview
sale 15% off
Preview
Standard

ISO 16364:2026 - Corrosion des métaux et alliages — Lignes directrices pour le contrôle de la corrosion galvanique

Release Date:10-Aug-2026
French language (16 pages)
sale 15% off
Preview
sale 15% off
Preview

Get Certified

Connect with accredited certification bodies for this standard

Element Materials Technology

Materials testing and product certification.

UKAS United Kingdom Verified

Inštitut za kovinske materiale in tehnologije

Institute of Metals and Technology. Materials testing, metallurgical analysis, NDT.

SA Slovenia Verified

Sponsored listings

Frequently Asked Questions

ISO 16364:2026 is a standard published by the International Organization for Standardization (ISO). Its full title is "Corrosion of metals and alloys — Guidelines for galvanic corrosion control". This standard covers: This document specifies standard methods for avoiding galvanic corrosion in the design stage and for determining whether actual corrosion damage was caused by galvanic corrosion. It also specifies guideline for standard methods for suppressing galvanic corrosion. This document also provides guidance for predicting galvanic corrosion in different environments (e.g. in water and in atmospheric and soil environments) by numerical calculation based on polarization data. This document does not establish the grounds for indexes related to safety or the loss of functions of materials in actual use. However, this document can be used to estimate the function maintenance life and safety maintenance life of these materials in advance. The responsibility for using the guideline rests with the reader.

This document specifies standard methods for avoiding galvanic corrosion in the design stage and for determining whether actual corrosion damage was caused by galvanic corrosion. It also specifies guideline for standard methods for suppressing galvanic corrosion. This document also provides guidance for predicting galvanic corrosion in different environments (e.g. in water and in atmospheric and soil environments) by numerical calculation based on polarization data. This document does not establish the grounds for indexes related to safety or the loss of functions of materials in actual use. However, this document can be used to estimate the function maintenance life and safety maintenance life of these materials in advance. The responsibility for using the guideline rests with the reader.

ISO 16364:2026 is classified under the following ICS (International Classification for Standards) categories: 77.060 - Corrosion of metals. The ICS classification helps identify the subject area and facilitates finding related standards.

ISO 16364:2026 is available in PDF format for immediate download after purchase. The document can be added to your cart and obtained through the secure checkout process. Digital delivery ensures instant access to the complete standard document.

Standards Content (Sample)

Contents

  • Introduction
  • 1 Scope
  • 2 Normative references
  • 3 Terms and definitions
  • 3.1 corrosion potential
  • 3.2 coupling potential
  • 3.3 electrolyte
  • 3.4 area ratio
  • 3.5 corrosion accelerate structure
  • 4 General principles
  • 4.1 General
  • 4.2 Material design
  • 4.3 Suppressing galvanic corrosion
  • 5 Test report
  • Annex A
  • 7 Ni-Cr-Mo alloy C
  • 9 Ni-Cr-Mo-Cu-Si alloy B
  • 19 Ni-Al bronze
  • 31 Pb-Sn solder (50/50)
  • Annex B
  • Annex C
  • 1. Galvanic couple 3. Test procedure
  • Bibliography

Introduction

Use of multi-materials (i.e. use of metal materials as well as ceramics, semiconductors, carbon fibre and resins in structures) is advancing rapidly in industrial fields like electronic components, automobiles, aircraft, plant systems and infrastructure, among others. This has increased the possibility of galvanic corrosion, heightening the necessity of a comprehensive, cross-sectorial guideline for galvanic corrosion suppression that includes materials and their environments. However, there are no clear provisions concerning galvanic corrosion or standards other than bolting of dissimilar materials. The boundary element method (BEM) and the finite element method (FEM) enable modelling and numerical calculation of galvanic corrosion. Simulations by these methods have progressed and are already used in practical applications. Moreover, accompanying the application of multi-materials such as carbon and other non-metallic materials eluted from ceramics, carbon fibre reinforced plastic (CFRP) or resins is related to galvanic corrosion. This galvanic corrosion has become a critical issue in automobiles, aircraft, etc. Under these circumstances, a cross-sectorial guideline on galvanic corrosion, with its many inherent issues, is necessary.

International Standard ISO 16364:2026(en) Corrosion of metals and alloys — Guidelines for galvanic corrosion control

1 Scope

This document specifies standard methods for avoiding galvanic corrosion in the design stage and for determining whether actual corrosion damage was caused by galvanic corrosion. It also specifies guideline for standard methods for suppressing galvanic corrosion.

This document also provides guidance for predicting galvanic corrosion in different environments (e.g. in water and in atmospheric and soil environments) by numerical calculation based on polarization data. This document does not establish the grounds for indexes related to safety or the loss of functions of materials in actual use. However, this document can be used to estimate the function maintenance life and safety maintenance life of these materials in advance. The responsibility for using the guideline rests with the reader.

2 Normative references

There are no normative references in this document.

3 Terms and definitions

For the purposes of this document, the following terms and definitions apply. ISO and IEC maintain terminology databases for use in standardization at the following addresses:

  • ISO Online browsing platform: available at https:// www .iso .org/ obp
  • IEC Electropedia: available at https:// www .electropedia .org/

3.1 corrosion potential

potential measured when materials A and B are immersed individually in the environmental electrolyte (3.3) concerned Note 1 to entry: Corrosion potential is given as either noble or base potential. Noble potential indicates a potential on the positive side. Base potential indicates a potential on the negative side.

3.2 coupling potential

potential measured when an electrical short circuit is established between materials A and B which are in contact with the electrolyte (3.3) concerned

3.3 electrolyte

ionically conductive liquid or solid medium covering the surfaces of material A and material B

3.4 area ratio

ratio of the area of material A with a base corrosion potential (3.1) and material B with a noble corrosion potential

ISO 16364:2026(en)

3.5 corrosion accelerate structure

structures where galvanic corrosion increases the corrosion (corrosion mass loss on the base side due to anodic reaction)

Note 1 to entry: The usual unit of corrosion is g/m .

EXAMPLE When the potential difference between metals is large or the anode area is small compared to the cathode.

4 General principles

4.1 General

This document provides guidance to minimise galvanic corrosion. Galvanic corrosion is caused by an electric current flow from a material A (anode) with a base potential to a material B (cathode) with a noble potential via an electrolyte and then returned to the base material A through conductive wiring, a conducting body or the material itself (see Annex A). This current causes galvanic corrosion and, as the current increases, the anodic current density on the surface of material A increases and the galvanic corrosion rate correspondingly rises. Galvanic corrosion is accelerated by electrical contact between materials with different electric potentials. The method of preventing galvanic corrosion involves reviewing the process and mitigation using a flowchart that includes one or more of the following:

a) materials designed for avoiding galvanic corrosion; b) evaluation method for determining whether actual corrosion damage was caused by galvanic corrosion; c) corrosion protection method for suppressing galvanic corrosion.

4.2 Material design

4.2.1 General

Figure 1 shows a material design flowchart for avoiding galvanic corrosion. It shows when material selection or, if possible, removal or change in electrolyte should be considered as a design change. It can also be used as an evaluation method for determining whether actual corrosion damage was caused by galvanic corrosion. The process is described in 4.2.2 to 4.2.5.

4.2.2 Conductive dissimilar materials

It may be verified whether conductive dissimilar materials are in electrical contact. In addition to direct contact, “electrical contact” also includes electrical continuity (conduction) by way of wiring, etc. In the absence of electrical continuity, galvanic corrosion does not take place between those materials.

4.2.3 Contact with a common electrolyte

It may be verified whether the dissimilar materials are in electrical contact and whether they are also in contact with a common electrolyte. This means verifying whether electrical continuity exists between the two materials and whether the two materials have also formed an external circuit that has electrical conduction by the electrolyte. If an electrolyte is not present, galvanic corrosion is avoided. In case of condensation which can lead to the presence of electrolyte, it is possible that the presence is only cyclical and therefore not permanently observable. It can be ascertained whether or not there is a risk of condensation.

ISO 16364:2026(en)

4.2.4 Corrosion accelerating structure

If dissimilar materials are in electrical contact and an electrolyte also exists between the materials, it may be verified whether there are factors that accelerate corrosion. Even in the case of dissimilar materials, if the potentials of the two materials are on approximately the same level in the electrolyte, galvanic corrosion is avoided. If the cathode/anode area ratio of the surfaces in contact with the electrolyte is sufficiently small, galvanic corrosion is suppressed. In addition, if the electrolyte has high resistance, the effective area ratio will differ from the apparent area ratio. Galvanic corrosion can be avoided in structures in which these corrosion-suppressing actions occur. Conversely, if these actions do not occur and a corrosion-accelerating structure is formed, galvanic corrosion can occur. Corrosion accelerate structure can be made by increasing the potential difference with time, increasing the cathode/anode area ratio with time or increasing the conductivity on the electrolyte with time. In such a case, the design of the non-contacted materials may be changed.

4.2.5 Design changes

The design may be changed by conducting a data search on galvanic corrosion, predictive calculations for galvanic corrosion or accelerated galvanic corrosion testing. Calculation methods of galvanic corrosion are outlined in Annex B. Typical test methods of galvanic corrosion are outlined in Annex C. In accelerated testing, the amount of corrosion and the corrosion rate may be evaluated by preparing galvanic corrosion test specimens and conducting a salt spray test or cyclic corrosion test. Alternatively, the amount of corrosion and the corrosion rate may be evaluated by preparing galvanic corrosion test specimens and measuring the galvanic current using a zero-shunt ammeter or electrochemical testing using the constant potential polarization method set to the coupling potential. In predictive calculations, the amount of corrosion and the corrosion rate may be predicted by either:

  • the FEM, the numerical simulation to solve corrosion related equations by dividing the geometry into finite elements;
  • the BEM, the numerical simulation to solve corrosion related equations by dividing the boundary into elements).

Corrosion may be evaluated quantitatively by either of these methods (see Annex B). In predictive calculations, it can be possible to consider diffusion of dissolved oxygen for cases where the cathodic reaction becomes rate-controlling and the effect of corrosion products that are influential to control both (cathodic and anodic) reactions. If the design is modified, it can be necessary to recommence the process beginning with the "Contact of dissimilar materials?" step (see Figure 1). Finally, when all the judgement items are confirmed as “No”, the design may be fixed.

ISO 16364:2026(en) Figure 1 — Material design flowchart

...

Contents

  • Introduction
  • 1 Domaine d’application
  • 2 Références normatives
  • 3 Termes et définitions
  • 3.1 potentiel de corrosion
  • 3.2 potentiel de couplage
  • 3.3 électrolyte
  • 3.4 rapport de surface
  • 3.5 structure accélérant la corrosion
  • 4 Principes généraux
  • 4.1 Généralités
  • 4.2 Conception des matériaux
  • 4.3 Suppression de la corrosion galvanique
  • 5 Rapport d’essai
  • Annexe A
  • Annexe B
  • Annexe C
  • 1. Couple galvanique 3. Procédure d’essai
  • 2. Conditions
  • Bibliographie

Introduction

L’usage de multi-matériaux (autrement dit le recours à des matériaux métalliques combinés à des céramiques, des semi-conducteurs, des fibres de carbones et des résines dans certaines structures) progresse rapidement dans divers secteurs industriels tels que les composants électroniques, l’automobile, l’aéronautique, les systèmes et les infrastructures destinés aux usines, pour n’en citer que quelques-uns. Cette tendance a accru le risque de corrosion galvanique et accentué la nécessité de disposer de lignes directrices trans-sectorielles détaillées pour la suppression de la corrosion galvanique, couvrant les matériaux et leurs environnements. Il n’existe toutefois aucune disposition claire concernant la corrosion galvanique ni aucune norme autre que celles abordant le boulonnage de matériaux dissemblables. La méthode des éléments de frontière (BEM) et la méthode des éléments finis (FEM) permettent de modéliser et de calculer numériquement la corrosion galvanique. Les simulations réalisées avec ces méthodes ont progressé et sont déjà employées dans des applications pratiques. De plus, l’accompagnement de l’application de multi-matériaux tels que le carbone et d’autres matériaux non métalliques obtenus à partir de céramiques, de polymères renforcés de fibres de carbone (PRFC) ou de résines peut influer sur la corrosion galvanique. Cette corrosion galvanique est devenue un problème crucial dans l’automobile, l’aéronautique… Dans ces circonstances, il est nécessaire de disposer de lignes directrices trans-sectorielles sur la corrosion galvanique et ses nombreux aspects inhérents.

Norme internationale ISO 16364:2026(fr) Corrosion des métaux et alliages — Lignes directrices pour le contrôle de la corrosion galvanique

1 Domaine d’application

Le présent document spécifie les méthodes normalisées permettant d’éviter la corrosion galvanique durant la phase de conception et de déterminer si un dommage de corrosion existant a été provoqué par la corrosion galvanique. Il donne également les lignes directrices des méthodes normalisées permettant de supprimer la corrosion galvanique.

Le présent document fournit aussi des recommandations pour prédire la corrosion galvanique dans différents environnements (par exemple dans l’eau ou dans les environnements atmosphériques et du sol) par des calculs numériques basés sur des données de polarisation. Le présent document ne définit pas les fondements des indices liés à la sécurité ou à la perte de fonctions des matériaux dans le cadre de leur utilisation réelle. Il peut toutefois servir à estimer à l’avance la durée de vie résiduelle des matériaux avec maintien des fonctions et la durée de vie résiduelle des matériaux en sécurité. Il est de la responsabilité du lecteur d’utiliser ces lignes directrices.

2 Références normatives

Le présent document ne contient aucune référence normative.

3 Termes et définitions

Pour les besoins du présent document, les termes et définitions suivants s’appliquent. L’ISO et l’IEC tiennent à jour des bases de données terminologiques destinées à être utilisées en normalisation, consultables aux adresses suivantes:

  • ISO Online browsing platform: disponible à l’adresse https:// www .iso .org/ obp
  • IEC Electropedia: disponible à l’adresse https:// www .electropedia .org/

3.1 potentiel de corrosion

potentiel mesuré lorsque deux matériaux A et B sont immergés individuellement dans l’électrolyte (3.3) environnemental concerné Note 1 à l'article: Le potentiel de corrosion est donné sous la forme d’un potentiel noble ou d’un potentiel de base. Un potentiel noble indique un potentiel du côté positif. Un potentiel de base indique un potentiel du côté négatif.

3.2 potentiel de couplage

potentiel mesuré lorsqu’un court-circuit électrique est établi entre deux matériaux A et B qui sont en contact avec l’électrolyte (3.3) concerné

3.3 électrolyte

milieu liquide ou solide conducteur d’ions et recouvrant la surface du matériau A et du matériau B

ISO 16364:2026(fr)

3.4 rapport de surface

rapport entre la surface d’un matériau A présentant un potentiel de corrosion (3.1) de base et un matériau B présentant un potentiel de corrosion noble

3.5 structure accélérant la corrosion

structures dans lesquelles la corrosion galvanique accroît la corrosion (perte de masse par corrosion sur le côté de base provoquée par une réaction anodique)

Note 1 à l'article: La corrosion est habituellement exprimée en g/m . EXEMPLE Lorsque la différence de potentiel entre métaux est grande ou lorsque la surface de l’anode est petite par rapport à celle de la cathode.

4 Principes généraux

4.1 Généralités

Le présent document fournit des recommandations pour réduire le plus possible la corrosion galvanique. La corrosion galvanique est causée par un courant électrique circulant d’un matériau A (anode) avec un potentiel de base à un matériau B (cathode) avec un potentiel noble via un électrolyte, puis retournant au matériau de base A par le biais d’un câblage conducteur, d’un corps conducteur ou du matériau lui-même (voir l’Annexe A). Ce courant provoque une corrosion galvanique et, à mesure que le courant augmente, la densité du courant anodique à la surface du matériau A augmente et le taux de corrosion galvanique augmente en conséquence. La corrosion galvanique est accélérée par le contact électrique entre des matériaux présentant des potentiels électriques différents.

La méthode permettant de prévenir la corrosion galvanique consiste à examiner le processus et les mesures d’atténuation à l’aide d’un organigramme comprenant un ou plusieurs des éléments suivants:

a) des matériaux conçus pour éviter la corrosion galvanique; b) une méthode d’évaluation permettant de déterminer si un dommage de corrosion existant est dû à la corrosion galvanique; c) une méthode de protection contre la corrosion permettant de supprimer la corrosion galvanique.

4.2 Conception des matériaux

4.2.1 Généralités

La Figure 1 montre un organigramme de la conception des matériaux permettant d’éviter la corrosion galvanique. Il indique quand il convient d’envisager de modifier la conception en changeant le choix des matériaux ou, si possible, en retirant ou en remplaçant l’électrolyte. Il peut également servir de méthode d’évaluation pour déterminer si un dommage de corrosion existant est dû à la corrosion galvanique. Le processus est décrit en 4.2.2 à 4.2.5.

4.2.2 Matériaux conducteurs dissemblables

Il est possible de vérifier si des matériaux conducteurs dissemblables sont en contact électrique. Outre un contact direct, le “contact électrique” implique également une continuité électrique (conduction) par le biais de câbles, etc. En l’absence de continuité électrique, aucune corrosion galvanique ne se produit entre ces matériaux.

ISO 16364:2026(fr)

4.2.3 Contact avec un électrolyte commun

Il est possible de vérifier si les matériaux dissemblables sont en contact électrique et s’ils sont également en contact avec un électrolyte commun. Il s’agit de vérifier s’il existe une continuité électrique entre les deux matériaux et si les deux matériaux forment aussi un circuit externe dont la conduction électrique est assurée par l’électrolyte. En l’absence d’électrolyte, la corrosion galvanique est évitée. En cas de condensation pouvant conduire à la présence d’électrolyte, il est possible que cette présence ne soit que cyclique et donc non observable en permanence. Il est possible de déterminer s’il existe ou non un risque de condensation.

4.2.4 Structure accélérant la corrosion

Si des matériaux dissemblables sont en contact électrique et si un électrolyte est également présent entre les matériaux, il est possible de vérifier s’il existe des facteurs qui accélèrent la corrosion. Même dans le cas de matériaux dissemblables, si les potentiels des deux matériaux sont à peu près du même niveau dans l’électrolyte, la corrosion galvanique est évitée. Si le rapport des surfaces cathode/anode en contact avec l’électrolyte est suffisamment faible, la corrosion galvanique est supprimée. En outre, si l’électrolyte présente une résistance élevée, le rapport de surface effectif sera différent du rapport de surface apparent. La corrosion galvanique peut être évitée dans les structures dans lesquelles sont mises en œuvre ces actions de suppression de la corrosion. Inversement, si ces actions ne sont pas mises en œuvre et si une configuration de structure accélérant la corrosion est formée, une corrosion galvanique peut se produire. Il est possible de créer une structure accélérant la corrosion en augmentant la différence de potentiel au cours du temps, en augmentant le rapport de surface cathode/anode au cours du temps ou en augmentant la conductivité de l’électrolyte au cours du temps. Dans ce cas, la conception des matériaux sans contact peut être modifiée.

4.2.5 Modifications de conception

La conception peut être modifiée en effectuant une recherche de données sur la corrosion galvanique, des calculs prédictifs de la corrosion galvanique ou des essais de corrosion galvanique accélérée. Les méthodes de calcul de la corrosion galvanique sont décrites à l’Annexe B. Les méthodes d’essai typiques de la corrosion galvanique figurent à l’Annexe C. Au cours d’essais accélérés, l’ampleur de la corrosion et la vitesse de corrosion peuvent être évaluées en préparant des éprouvettes pour la corrosion galvanique et en effectuant un essai au brouillard salin ou un essai de corrosion cyclique. Il est également possible d’évaluer l’ampleur de la corrosion et la vitesse de corrosion en préparant des éprouvettes pour la corrosion galvanique et en mesurant le courant galvanique à l’aide d’un ampèremètre à shunt nul ou d’un essai électrochimique selon la méthode de la polarisation à potentiel constant réglée sur le potentiel de couplage. Dans les calculs prédictifs, l’ampleur de la corrosion et la vitesse de corrosion peuvent être prédites par l’une ou l’autre des méthodes suivantes:

  • la FEM, avec une simulation numérique permettant de résoudre les équations de la corrosion en divisant la géométrie en éléments finis;
  • la BEM, avec une simulation numérique permettant de résoudre les équations de la corrosion en divisant la frontière en éléments.

La corrosion peut être évaluée quantitativement par l’une ou l’autre de ces méthodes (voir l’Annexe B). Dans les calculs prédictifs, il est possible de prendre en compte la diffusion de l’oxygène dissous dans les cas où la réaction cathodique devient cinétiquement limitante et l’effet des produits de corrosion qui influent sur le contrôle des deux réactions (cathodique et anodique). Si la conception est modifiée, il peut s’avérer nécessaire de recommencer le processus en commençant par l’étape “Contact entre matériaux dissemblables?” (voir Figure 1). Pour finir, lorsqu’il est confirmé que tous les éléments d’appréciation correspondent à “non”, la conception peut être figée.

...