Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate [Metric]

SCOPE
1.1 This specification covers aluminum and aluminum alloy flat sheet, coiled sheet, and plate, in the alloys (Note 1) and tempers shown in, Tables 2 and 3 in the following finishes:
1.1.1 Plate in all alloys and sheet in heat-treatable alloys: mill finish.
1.1.2 Sheet in nonheat-treatable alloys: mill finish, one-side bright mill finish, standard one-side bright finish, and standard two-sides bright finish.
1.2 Alloy and temper designations are in accordance with ANSI H35.1M. The equivalent Unified Numbering System alloy designations are those of Table 1 preceded by A9, for example, A91100 for aluminum 1100 in accordance with Practice E 527.
Note 1—Throughout this specification, use of the term alloyin the general sense includes aluminum as well as aluminum alloy.
Note 2—See Specification B 632/B 632M for Tread Plate.
1.3 This specification is the metric counterpart of Specification B 209.
1.4 For acceptance criteria for inclusion of new aluminum and aluminum alloys in this specification, see Annex A2.

General Information

Status
Historical
Publication Date
09-Apr-2002
Current Stage
Ref Project

Relations

Buy Standard

Technical specification
ASTM B209M-02 - Standard Specification for Aluminum and Aluminum-Alloy Sheet and Plate [Metric]
English language
26 pages
sale 15% off
Preview
sale 15% off
Preview

Standards Content (Sample)

NOTICE: This standard has either been superseded and replaced by a new version or discontinued.
Contact ASTM International (www.astm.org) for the latest information.
Designation: B 209M – 02
METRIC
Standard Specification for
1
Aluminum and Aluminum-Alloy Sheet and Plate [Metric]
This standard is issued under the fixed designation B 209M; the number immediately following the designation indicates the year of
original adoption or, in the case of revision, the year of last revision. A number in parentheses indicates the year of last reapproval. A
superscript epsilon (e) indicates an editorial change since the last revision or reapproval.
This standard has been approved for use by agencies of the Department of Defense.
2
1. Scope * Alloy Wrought Products for Aerospace Applications
B 632/B 632M Specification for Aluminum-Alloy Rolled
1.1 This specification covers aluminum and aluminum alloy
2
Tread Plate
flat sheet, coiled sheet, and plate, in the alloys (Note 1) and
B 660 Practices for Packaging/Packing of Aluminum and
tempers shown inTables 2 and 3, and in the following finishes:
2
Magnesium Products
1.1.1 Plate in all alloys and sheet in heat-treatable alloys:
B 666/B 666M Practice for Identification Marking of Alu-
mill finish.
2
minum and Magnesium Products
1.1.2 Sheet in nonheat-treatable alloys: mill finish, one-side
B 918 Practice for Heat Treatment of Wrought Aluminum
bright mill finish, standard one-side bright finish, and standard
2
Alloys
two-sides bright finish.
3
E 3 Methods of Preparation of Metallographic Specimens
1.2 Alloy and temper designations are in accordance with
E 29 Practice for Using Significant Digits in Test Data to
ANSI H35.1M. The equivalent Unified Numbering System
4
Determine Conformance with Specifications
alloy designations are those of Table 1 preceded by A9, for
E 34 Test Methods for Chemical Analysis of Aluminum and
example, A91100 for aluminum 1100 in accordance with
5
Aluminum-Base Alloys
Practice E 527.
E 55 Practice for Sampling Wrought Nonferrous Metals and
NOTE 1—Throughout this specification, use of the term alloy in the 5
Alloys for Determination of Chemical Composition
general sense includes aluminum as well as aluminum alloy.
3
E 290 Test Method for Bend Test for Ductility
NOTE 2—See Specification B 632/B 632M for Tread Plate.
3
E 407 Practice for Microetching Metals and Alloys
6
1.3 This specification is the metric counterpart of Specifi-
E 527 Practice for Numbering Metals and Alloys (UNS)
cation B 209.
E 607 Test Method for Optical Emission Spectrometric
1.4 For acceptance criteria for inclusion of new aluminum
Analysis of Aluminum and Aluminum Alloys by the
5
and aluminum alloys in this specification, see Annex A2.
Point-to-Plane Technique, Nitrogen Atmosphere
E 716 Practices for Sampling Aluminum and Aluminum
2. Referenced Documents
5
Alloys for Spectrochemical Analysis
2.1 The following documents of the issue in effect on the
E 1004 Practice for Determining Electrical Conductivity
date of material purchase, unless otherwise noted, form a part 7
Using the Electromagnetic Eddy-Current Method
of this specification to the extent referenced herein:
E 1251 Test Method for Optical Emission Spectrometric
2.2 ASTM Standards:
Analysis of Aluminum and Aluminum Alloys by the Argon
B 209 Specification for Aluminum and Aluminum-Alloy
Atmosphere, Point-to-Plane, Unipolar Self-Initiating Ca-
2
Sheet and Plate 5
pacitor Discharge
B 548 Method for Ultrasonic Inspection of Aluminum-
G 34 Test Method for Exfoliation Corrosion Susceptibility
2
Alloy Plate for Pressure Vessels
in 2XXX and 7XXX Series Aluminum Alloys (EXCO
B 557M Test Methods for Tension Testing Wrought and 8,9
Test)
2
Cast Aluminum- and Magnesium-Alloy Products [Metric]
B 594 Practice for Ultrasonic Inspection of Aluminum-
3
Annual Book of ASTM Standards, Vol 03.01.
4
Annual Book of ASTM Standards, Vol 14.02.
1 5
This specification is under the jurisdiction of ASTM Committee B07 on Light Annual Book of ASTM Standards, Vol 03.05.
6
Metals and Alloys and is the direct responsibility of Subcommittee B07.03 on Annual Book of ASTM Standards, Vol 01.01.
7
Aluminum Alloy Wrought Products. Annual Book of ASTM Standards, Vol 03.03.
8
Current edition approved Apr. 10, 2002. Published June 2002. Originally The applicable edition in the use of this specification is G34 – 72—available in
published as B 209M – 78. Last previous edition B 209M – 01. the gray pages of the Annual Book of ASTM Standards, Vol 02.02.
2 9
Annual Book of ASTM Standards, Vol 02.02. Annual Book of ASTM Standards, Vol 03.02.
*A Summary of Changes section appears at the end of this standard.
Copyright © ASTM International, 100 Barr Harbor Drive, PO Box C700, West Conshohocken, PA 19428-2959, United States.
1

---------------------- Page: 1 ----------------------
NOTICE: This standard has either been superseded and replaced by a new version or discontinued.
Contact ASTM International (www.astm.org) for the latest information.
B 209M
A,B,C
TABLE 1 Chemical Composition Limits
...