Status
Not Published
Public Enquiry End Date
30-Sep-2026
Current Stage
4020 - Public enquire (PE) (Adopted Project)
Start Date
04-Aug-2026
Due Date
22-Dec-2026
Completion Date
29-Sep-2026

Buy Documents

Draft

oSIST prEN IEC 60243-2:2026

English language (12 pages)
Preview
Preview
e-Library read for
×1 day

oSIST prEN IEC 60243-2:2026 is a draft IEC/CENELEC standard for measuring the electric strength of solid insulating materials under direct voltage. It adds requirements to the basic IEC 60243 test method so laboratories, manufacturers, and test engineers can run comparable d.c. breakdown tests and report the results in a consistent way.

What does oSIST prEN IEC 60243-2:2026 specify?

oSIST prEN IEC 60243-2:2026 specifies the additional requirements for determining the electric strength of solid insulating materials under direct voltage stress. It is read together with IEC 60243-1:2013, which provides the base test method.

The document is organized into clauses on scope, normative references, terms and definitions, the significance of the test, electrodes and test specimens, conditioning, surrounding medium, electrical apparatus, procedure, mode of voltage increase, breakdown criterion, number of tests, and report.

What are the key requirements of oSIST prEN IEC 60243-2:2026?

Clause 4 explains why d.c. tests behave differently from a.c. tests. The electric field in non-homogeneous specimens can change with the rate of voltage rise, and currents such as capacitive current, absorption current, leakage current, and sometimes partial discharge current can appear. In practice, this means the same material can give different breakdown results depending on how the voltage is applied.

Clause 5 uses the electrode configurations and specimen shapes from IEC 60243-1:2013. This keeps the d.c. test aligned with the main series, so users do not need a separate specimen design unless a product standard says otherwise.

Clause 6 requires conditioning of specimens for at least 24 h at (23 ± 2) °C and (50 ± 5) % relative humidity, unless another condition is specified or agreed. The specimens are shorted and grounded during conditioning. This matters because temperature and moisture can shift the measured electric strength.

Clause 7 requires a surrounding medium selected to prevent flashover and limit unwanted effects on the material under test. Liquids, air at elevated temperature, or solid casting materials may be used depending on the specimen and test purpose. For liquid tests, an immersion test checks compatibility between the liquid and the specimen material, and the mass change limit is given in the clause.

Clause 8 sets the electrical apparatus requirements. The voltage source must allow positive or negative polarity, keep ripple and transient content low, control the rate of voltage rise within tolerance, and include current interruption and current-limiting provisions. For large specimens, the document also requires discharge and earthing measures so stored charge does not distort the result or create a safety hazard.

Clause 10 allows the voltage to be applied using the short-time, slow rate-of-rise, very slow rate-of-rise, or proof-test modes defined in IEC 60243-1:2013. Clause 11 treats breakdown as a sudden current increase or as current reaching a specified value. In practice, the test report must show which breakdown criterion was used.

Clause 13 defines the reporting items. The report records the material identification, specimen preparation, polarity, median electric strength or breakdown voltage, thickness, surrounding medium, electrode system, voltage mode, individual results, test environment, conditioning treatment, and the type and position of breakdown. That makes the result traceable and easier to compare between laboratories.

What terms does oSIST prEN IEC 60243-2:2026 define?

The terms and definitions in IEC 60243-1:2013 apply, and the document uses several technical concepts in a specific way.

  • Electric strength - the electric stress at which a specimen breaks down under the specified test conditions.
  • Breakdown - failure of the specimen, identified here by a sudden current rise or by current exceeding a set value.
  • Surrounding medium - the air, liquid, or casting material around the specimen during test.
  • Rate of voltage rise - how fast the applied voltage increases during the test, which affects d.c. field distribution.
  • Immersion test - the compatibility check used to see whether a liquid changes the specimen material before testing.
  • Current-limiting resistance - a series resistance used to protect the source and reduce electrode damage at breakdown.
  • Polarity - whether the applied d.c. test voltage is positive or negative.

Who uses oSIST prEN IEC 60243-2:2026?

oSIST prEN IEC 60243-2:2026 is used by laboratories that measure dielectric breakdown, by manufacturers of insulating materials, and by quality teams that need test results for product release or qualification. It also supports engineers who design and compare solid insulation systems for electrical equipment. Test and conformity assessment bodies use it to make sure d.c. electric strength results are obtained under a defined and repeatable method.

What changed in oSIST prEN IEC 60243-2:2026 from the previous edition?

oSIST prEN IEC 60243-2:2026 cancels and replaces the 3rd edition published in 2013. The stated technical changes are:

  • clauses 6 and 7 were rewritten using requirements from IEC 60243-1
  • the text in clauses 6 and 7 was updated for d.c. testing needs
  • the test voltage source specification was harmonized with IEC 60060-1

Which standards are used with oSIST prEN IEC 60243-2:2026?

  • IEC 60243-1:2013 - the base part that provides the general test method, specimen handling, procedure, breakdown criterion, and reporting structure.
  • IEC 60296 - gives requirements for mineral insulating oils used as a liquid surrounding medium.
  • IEC 61099 - gives specifications for unused synthetic organic esters used as insulating liquids.
  • IEC 60060-1 - used as the reference for harmonizing the test voltage source requirements.

What does the oSIST prEN IEC 60243-2:2026 document contain?

The document contains a foreword, an introduction, and 13 clauses covering the full d.c. test workflow from specimen conditioning to reporting. It includes a detailed immersion test procedure for checking whether a liquid is compatible with the specimen material before testing. Clause 8 describes the test power supply, voltage measurement, charge removal, and current-limiting arrangements. Clause 13 lists the data that should appear in the report, including test polarity, individual breakdown values, and the test environment.

Relations

Effective Date
27-Sep-2022

Buy Documents

Draft

oSIST prEN IEC 60243-2:2026

English language (12 pages)
Preview
Preview
e-Library read for
×1 day

Get Certified

Connect with accredited certification bodies for this standard

IMQ S.p.A. (Certification)

Italian electrical product certification.

ACCREDIA Italy Verified

SLG Prüf- und Zertifizierungs GmbH

German testing and certification body.

DAKKS Germany Verified

UL Solutions

Global safety science company with testing, inspection and certification.

ANAB United States Verified

Sponsored listings

Frequently Asked Questions

oSIST prEN IEC 60243-2:2026 is a draft published by the Slovenian Institute for Standardization (SIST). Its full title is "Electric strength of insulating materials - Test methods - Part 2: Additional requirements for tests using direct voltage". This standard covers: Electric strength of insulating materials - Test methods - Part 2: Additional requirements for tests using direct voltage

Electric strength of insulating materials - Test methods - Part 2: Additional requirements for tests using direct voltage

oSIST prEN IEC 60243-2:2026 is classified under the following ICS (International Classification for Standards) categories: 17.220.99 - Other standards related to electricity and magnetism; 29.035.01 - Insulating materials in general. The ICS classification helps identify the subject area and facilitates finding related standards.

oSIST prEN IEC 60243-2:2026 has the following relationships with other standards: It is inter standard links to SIST EN 60243-2:2014. Understanding these relationships helps ensure you are using the most current and applicable version of the standard.

oSIST prEN IEC 60243-2:2026 is available in PDF format for immediate download after purchase. The document can be added to your cart and obtained through the secure checkout process. Digital delivery ensures instant access to the complete standard document.

Standards Content (Sample)

Contents

  • 1 Scope
  • 2 Normative references
  • 3 Terms and definitions
  • 4 Significance of the test
  • 5 Electrodes and test specimens
  • 6 Conditioning before tests
  • 7 Surrounding medium
  • 7.1 General
  • 7.2 Tests in air at elevated temperature
  • 7.3 Test in liquids
  • 7.4 Tests in solid casting materials
  • 8 Electrical apparatus
  • 8.1 Voltage source
  • 8.2 Voltage measurement
  • 9 Procedure
  • 10 Mode of increase of voltage
  • 11 Criterion of breakdown
  • 12 Number of tests
  • 13 Report
  • Bibliography

INTRODUCTION This document describes the evaluation of eelectric strength under direct voltage stress for determining the performance of solid insulating materials.

oSIST prEN IEC 60243-2:2026

1 Scope

This part of IEC 60243 gives requirements additional to those in IEC 60243-1:2013 for the determination of the electric strength of solid insulating materials under direct voltage stress.

2 Normative references

The following documents are referred to in the text in such a way that some or all of their content constitutes requirements of this document. For dated references, only the edition cited applies. For undated references, the latest edition of the referenced document (including any amendments) applies.

IEC 60243-1:2013, Electric strength of insulating materials – Test methods – Part 1: Tests at power frequencies IEC 60296, Fluids for electrotechnical applications – Mineral insulating oils for electrical equipment IEC 61099, Insulating liquids - Specifications for unused synthetic organic esters for electrical purposes

3 Terms and definitions

For the purposes of this document, the terms and definitions in IEC 60243-1:2013 apply.

4 Significance of the test

In addition to the requirements of IEC 60243-1:2013, Clause 4, the following points shall be considered when using direct-voltage tests.

For a non-homogeneous test specimen, with alternating voltage, the distribution of electric field within the test specimen is determined by impedance (largely capacitive). With an increasing direct voltage, the electric field distribution may still be largely capacitive but depends partly on the rate of voltage increase. The resistive electric field distribution, after constant voltage application, represents the steady-state condition.

The electric field distribution depends on the material properties and on the rate of the increasing test voltage, which will affect the breakdown behavior as a combination of alternating and direct voltage breakdown.

Upon direct voltage application, the following currents result: the capacitive current, the electric absorption current, the leakage current, and, in some cases, partial discharge currents. In addition, for materials with dissimilar layers or discontinuities, the voltage distribution across the test specimen is also influenced, as a result of interfacial polarization, by charges of opposite polarity, which may accumulate on the two sides of the interface and create local fields sufficiently strong to produce partial discharges and/or breakdown of the test specimens. For most materials, the d.c. breakdown voltage is higher than the peak value of the power - frequency breakdown voltage; for many materials, particularly those that are nonhomogeneous, the d.c. breakdown voltage will be three times higher than the a.c. brea kdown voltage or even more.

oSIST prEN IEC 60243-2:2026

5 Electrodes and test specimens

For the purposes of this standard, the electrode configurations and shape of test specimen of IEC 60243-1:2013, Clause 5 are applicable.

6 Conditioning before tests

The electric strength of insulating materials varies with temperature and moisture content. If not otherwise specified by the relevant product standard, of unless other conditions are agreed upon, specimens shall be conditioned for not less than 24 h at (23 ± 2) °C, (50 ± 5) % relative humidity.During this conditioning period the samples must be shorted and grounded.

7 Surrounding medium

7.1 General

Materials should be tested in a surrounding medium selected to prevent flashover. Suitable materials may be liquids (e.g. transformer oil according to IEC 60296 , silicone fluid according to IEC 60836 [1] or ester fluid according to IEC 61099 ) or appropriate casting materials. Specimens having relatively low breakdown values may be tested in air, particularly if the tests are to be made at elevated temperature.

Select a medium which has minimum deleterious effect on the material under test. The effect of the ambient medium on the results may be great, particularly in the case of absorbent materials such as paper and pressboard, and it is essential that procedures for specimen preparation define fully all necessary steps (e.g. drying and impregnation), and the condition of the ambient medium during test.

Sufficient time shall be allowed for the specimen and the electrodes to attain the required temperature, but some materials may be affected by prolonged exposure to high temperatures. If it is intended that the tests evaluate the behaviour of a material in another medium, that medium may be used.

...