Aerospace series - Cadmium plating of steels with specified tensile strength <= 1450 MPa, copper, copper alloys and nickel alloys

This standard specifies the electrolytic cadmium plating of parts in steels of tensile strength Rm (max.)

Luft- und Raumfahrt - Verkadmen von Stählen mit einer Zugfestigkeit <= 1 450 MPa, von Kupfer, von Kupferlegierungen und von Nickellegierungen

Diese Norm legt das elektrolytische Verkadmen von Teilen aus Stahl mit einer Zugfestigkeit Rm (max.)

Série aérospatiale - Cadmiage électrolytique des aciers de résistance <= 1 450 MPa, du cuivre, des alliages de cuivre et des alliages de nickel

La présente norme spécifie le cadmiage électrolytique des pièces en acier de résistance en traction Rm (max.)

Aerospace series - Cadmium plating of steels with specified tensile strength <= 1450 MPa, copper, copper alloys and nickel alloys

General Information

Status
Withdrawn
Publication Date
18-Nov-1997
Withdrawal Date
19-Oct-2010
Technical Committee
ASD/MAT - Materials
Drafting Committee
ASD/MAT - Materials
Current Stage
9960 - Withdrawal effective - Withdrawal
Start Date
20-Oct-2010
Completion Date
20-Oct-2010

Relations

Effective Date
23-Oct-2010

Get Certified

Connect with accredited certification bodies for this standard

National Aerospace and Defense Contractors Accreditation Program (NADCAP)

Global cooperative program for special process quality in aerospace.

ANAB United States Verified

NSF-ISR

NSF International Strategic Registrations.

ANAB United States Verified

Orion Registrar Inc.

US-based certification body for management systems.

ANAB United States Verified

Sponsored listings

Frequently Asked Questions

EN 2133:1997 is a standard published by the European Committee for Standardization (CEN). Its full title is "Aerospace series - Cadmium plating of steels with specified tensile strength <= 1450 MPa, copper, copper alloys and nickel alloys". This standard covers: This standard specifies the electrolytic cadmium plating of parts in steels of tensile strength Rm (max.) </= 1450 MPa, copper, copper alloys and nickel alloys, the temperature in service of which does not exceed 235 °C. This standardd is applicable whenever referenced.

This standard specifies the electrolytic cadmium plating of parts in steels of tensile strength Rm (max.) </= 1450 MPa, copper, copper alloys and nickel alloys, the temperature in service of which does not exceed 235 °C. This standardd is applicable whenever referenced.

EN 2133:1997 is classified under the following ICS (International Classification for Standards) categories: 49.040 - Coatings and related processes used in aerospace industry. The ICS classification helps identify the subject area and facilitates finding related standards.

EN 2133:1997 has the following relationships with other standards: It is inter standard links to EN 2133:2010. Understanding these relationships helps ensure you are using the most current and applicable version of the standard.

EN 2133:1997 is available in PDF format for immediate download after purchase. The document can be added to your cart and obtained through the secure checkout process. Digital delivery ensures instant access to the complete standard document.

Standards Content (Sample)


2003-01.Slovenski inštitut za standardizacijo. Razmnoževanje celote ali delov tega standarda ni dovoljeno.Aerospace series - Cadmium plating of steels with specified tensile strength <= 1450 MPa, copper, copper alloys and nickel alloysLuft- und Raumfahrt - Verkadmen von Stählen mit einer Zugfestigkeit <= 1 450 MPa, von Kupfer, von Kupferlegierungen und von NickellegierungenSérie aérospatiale - Cadmiage électrolytique des aciers de résistance <= 1 450 MPa, du cuivre, des alliages de cuivre et des alliages de nickelAerospace series - Cadmium plating of steels with specified tensile strength <= 1450 MPa
...

Questions, Comments and Discussion

Ask us and Technical Secretary will try to provide an answer. You can facilitate discussion about the standard in here.

Loading comments...